Fives teams with National Research Council of Canada

0
4948

The National Research Council of Canada (NRC) and Fives are working together to develop an advanced profilometer that will provide faster and more accurate part inspection in aerospace manufacturing.

As the aerospace industry in Canada and around the world continues to increase its use of automated composite manufacturing techniques to produce large aircraft components, the industry is eager to find solutions to manufacture reliable, safe, and cost-effective composite structures.

Based on an innovative optical technology, the advanced profilometer for composite placement shows considerable advantages over existing inspection technologies used for the same purposes. This groundbreaking in-process inspection technology will help manufacturers meet strict standards by providing superior measuring information without limiting the process functionality. These faster, better measurements will speed up manufacturing processes, reduce the risk of errors, and help composite manufacturers be more competitive.

Fives has already started the last testing stage of the next-generation profilometer with customers and expects to begin commercializing the technology before the end of 2019. The NRC and Fives will continue to work together to advance this technology and bring innovative manufacturing solutions to the aerospace industry.

Manufacturing makes up nearly half of Canada’s aerospace sector. Canada is home to more than 700 aerospace companies employing over 85,000 skilled professionals. The aerospace industry contributed $12.6 billion to Canadian Gross Domestic Product (GDP) in 2017.

Fives designs and supplies machines, process equipment and production lines for various industrial sectors and is a major supplier of composite manufacturing equipment to the aerospace industry.