PRODUCT SHOWCASE: New Coating Enhances Seco Tool Milling Cutters

0
5096

Seco Tools has enhanced the performance of its entire Turbo Mill family of square shoulder milling cutters through a new nickel-based surface coating that approaches HV700 on the pre-hardened cutter bodies for longer life, better tolerances, and a more durable surface. For the user, this translates into increased reliability, higher precision machining, and better chip evacuation and control. Seco’s Turbo Mill offering is a comprehensive and versatile square shoulder milling product line that can slot, ramp, contour, plunge, pocket mill, and perform both circular and helical interpolation. There is a choice of 13 carbide grades, three PCD tipped grades and five geometries suited for a variety of materials including steel, stainless steel, cast iron, hardened materials, high-temperature alloys, and nonferrous materials. Go to [www.secotools.com].