Dillon full grip jaws are machined from 6061 extruded aluminum for increased strength. (Courtesy: Dillon Manufacturing)

Dillon full grip jaws, machined from 6061 extruded aluminum for increased strength, are now available up to 28 inches in diameter.

Machining from bar stock eliminates the porosity inherent with large diameter aluminum castings, providing a stronger and more reliable workholding product. These jaws can be modified to heights of 10” and widths that extend beyond the chuck face diameter, thus increasing the chuck’s capacity.

Dillon chuck jaws can provide both standard and special pie jaws in 1.5mm x 60°, 3.0mm x 60°, 1/16th x 90°, and 3/32 x 90° serrations, American standard and metric tongue and groove, and acme and square serrated key type mounting interfaces. They are also available in 1018 CR steel and cast iron. Most standard and special jaw modification have less than a two-week lead time.

Dillon chuck jaw products are made in the USA in an ISO 9000-2015 registered facility.
Dillon Manufacturing, Inc. manufactures a complete line of standard and custom workholding solutions including chuck jaws, chucks, vises, soft jaws, hard jaws, collet pads, and more. It manufactures jaws using 1018, 1045, 4140, 8620, A-2, and 6061 aluminum. Dillon Manufacturing is ISO 9000-2015 registered.