Ovako introduces Hybrid Steel®

0
5230

At the Euromat 2017 congress, Ovako introduced Hybrid Steel, a new innovative steel family that challenges traditional steel categorizations. It offers properties of tool steel, maraging steel, and stainless steel, combined with the production economy of engineering steel. It is set to enable customers to achieve exceptional performance and help reduce production costs.

“We are convinced that our hybrid steel is a groundbreaking innovation for the steel industry,” said Marcus Hedblom, president and CEO at Ovako. “By using a new alloying philosophy, we have created a steel that has three times the yield and tensile strength of conventional steel at temperatures up to 500°C. These properties are ideal for a wide variety of highly-stressed applications such as engine components, bearings, and tools for various purposes.”

Because Hybrid Steel develops its full properties through heat treatment at temperatures that cause a very low distortion, manufacturers will be able to adopt new, more efficient processes that eliminate a number of stages. For example, a component might be machined to its final dimensions in a softer condition and then heat treated to achieve its full strength, a route that could offer a significant reduction in manufacturing cost and complexity.

Hybrid Steel takes its name from the simultaneous hardening by both carbides and intermetallic precipitations.

”In this hybrid steel, you combine both mechanisms and indeed the properties are very good, and in particular the material maintains them at elevated temperatures,” said John Ågren, professor in physical metallurgy at Royal Institute of Technology, Stockholm.

The development of Hybrid Steel has been carried out at Ovako’s R&D facilities in Hofors. Prototype test programs are already under way with a number of component manufacturers.