Gear deburring is a process that has changed substantially over the past 10 years. There have been advancements in the types of tools used for deburring operations and the development of “wet” machines, automatic load and unload, automatic part transfer and turnover, and vision systems for part identification, etc.
Three types of tools are used in the gear deburring process, including grinding wheels, brushes, and carbide tools. A discussion of each method is as follows.
Grinding Wheels
There are many wheel grits available, from 320 grit for small burrs and light chamfers, to 57 grit for large burrs and heavy chamfers, with numerous grit sizes in between. Grinding wheels will usually provide the required cosmetic appearance for a deburred gear. Setting up the grinding wheel is critical for good wheel life and consistent chamfers. The point of contact for the grinding wheel should be equal to the approach angle of the grinding head. For example, set a 45° approach angle for the grinding head with a protractor. Next, draw a line through the center of the grinding wheel followed by a line drawn 45° to the first line. The contact point between the gear and the grinding wheel should be at the 45° line (see Figure 1, which shows a gear deburred with a grinding wheel). This setup will result in optimum performance of the grinding wheel.
The size of the chamfer attainable is determined by the size of the burr to be removed from the part. Further, three additional factors that affect chamfer size are wheel grit size, speed of the work spindle, and the amount of pressure applied to the part by the grinding wheel. Grinding wheel speed is noted on the grinding wheel, and it is usually 15,000 to 18,000 RPM. The grinding wheels used most often are aluminum oxide.
Brushes
Parts with small burrs can be effectively deburred with a brush (see Figure 2). Two types of brushes are used for deburring operations, those being wire and nylon. Wire brushes are made with straight, crimped, or knotted bristles. The wire diameter and length will determine how aggressively the brush will deburr. Nylon brushes can be impregnated with either aluminum oxide or silicon carbide, with grit size ranging from 80 to 400. The specific application will determine which type of brush is required. In applications where a heavy burr is to be removed with a grinding wheel or carbide tool, a brush is often used as a secondary process for removing small burrs created by the first process.
Carbide Tools
The use of carbide deburring tools is a relatively new development. There are three advantages to using carbide tools:
• Reduced deburring time. The carbide tools can run at 40,000 RPM, vs. 15,000 to 18,000 RPM for grinding wheels.
• Reduced setup time, because there is no need to establish an approach angle as with a grinding wheel (see Figure 3).
• Ability to deburr cluster gears, or gears having the root of the tooth close to the gear shaft or hub.
Deburring Machine Features
- The deburring process is accomplished with floating-style deburring heads having variable RPM air motors or turbines. The floating heads have air-operated, adjustable counterweights for adjusting the pressure applied to the part being deburred.
The floating heads can use grinding wheels, brushes, or carbide tools, and change-over from one to the other can be accomplished in a matter of minutes, providing versatility for doing a number of different parts on one machine.
Dry and Wet Machines
The dry machine is so named because the deburring operation is performed dry. Usually, these machines are equipped with a dust collection system. Deburring on a dry machine is best accomplished if the parts are clean and dry prior to deburring. With a wet machine, a non-foaming rust preventative is applied to the part during the deburring process (see Figure 4).
The wet machine is becoming quite popular. It costs more than the dry machine, but there are many advantages:
• Increased tool life
• Parts leave the machine clean and dry with rust preventative applied (see Figure 5), eliminating the need for extra handling and equipment for post-deburring operations
• The dust and slivers generated by the deburring process are eliminated
• The burn marks on gear teeth are eliminatedAutomation
• The productivity of a deburring machine can be greatly increased by the addition of various forms of automation. They include:
• Power conveyors for the automatic loading and unloading of parts
• Programmable servos for positioning the deburring heads
• “Pick and place” units, or robots, for transferring the parts from the load conveyor to the work-holding chuck (power-operated clamping) and for removing the deburred parts from the chuck and placing them on the unload conveyor (see Figure 6)
• Turnover units to facilitate deburring of two sides of a part in an automated system
• Vision systems for identifying where the burr is located on a part (see Figure 7)
In addition to increased productivity, the flexibility provided by these automation devices permits efficient processing of a variety of parts through one machine because change-over from one part to another is not complicated and can be done quickly. Therefore, one machine with automation can efficiently deburr a number of parts, reducing the need for multiple machines (see Figure 8 and Figure 9).