Induction Gear Hardening: Part 2

This is the second installment of a two-part article on induction hardening of gears and gear-like components. Part 1 was […]

Fatigue Performance and Cleanliness of Carburizing Steels for Gears

The cleanliness of steels used for gears is of great importance when looking to improve their life or increase loads. […]

Extending gear life in demanding applications

Although gears and other precision components are generally made of hardened steel or metal alloys, those used in high load […]

Advanced Thermal Processing for Enhanced Gear Tribology

Abstract Vast empirical knowledge accumulated over centuries, in conjunction with recent advances in the areas of material science, tribology, and […]

An Experimental and Analytical Comparison of the Noise Generated by Gears of Austempered Ductile Iron (ADI) and Steel Materials

Over the years, there have been many claims made concerning the relative noise performance of austempered ductile iron (ADI) versus […]

All Metals & Forge Group

All Metals & Forge Group is an ISO9001:2008, AS/EN9100:2009 Rev. C manufacturer dedicated to providing its customers with the quickest […]

IMT Forge Group

IMT Forge provides world-class, seamlessly integrated, single source closed-die forging service to customers across North America and around the world. […]

McInnes Rolled Rings

At McInnes, seamless describes more than just our rings. McInnes Rolled Rings, located in Erie, Pennsylvania, started operations in 1992. […]

Allied Sinterings, Inc.

Allied Sinterings is a recognized world leader in the manufacture of custom-engineered powder metal products for small applications, including small […]

P & G Machine & Supply Co., Inc.

P & G Machine & Supply Company, Inc. is a well-established, service driven, sales and manufacturing company which gives customers […]

Niagara Gear Corporation

Located in Buffalo, NY, Niagara Gear Corporation is an established, world class manufacturer of precision ground, spur, helical and pump gears. Purchased in 1974 […]

National Bronze & Metals, Inc.

National Bronze & Metals, Inc. (NBM) based out of Houston, Texas maintains an inventory in excess of 10 million pounds […]

Ka-Wood Gear & Machine Co.

KA-WOOD GEAR & MACHINE CO. is a leader in gear and spline manufacturing.  We manufacture precision products for a diverse […]

Clifford-Jacobs Forging Co.

OUR VISION. At Clifford-Jacobs we strive to form true “partnerships of value” with every customer. We are able to do […]

Contact Ratio Optimization of Powder-Metal Gears

Powder metal (PM) alloys are becoming more of a solution for high-performance gears, not only because of part price but […]

Case Study: How Advanced Gearbox Testing Drove the Need for the Lost Foam Casting Process

For decades, powertrain test systems incorporated custom test stand gearboxes constructed with fabricated gearbox housings. In some cases, fabricated housings […]

Gear Design Relevant Cleanness Metrics

The “Metallurgical Specifications for Steel Gearing” information sheet (AGMA 923-B05) [1] details non-metallic inclusion limits to meet AGMA grade expectations […]

Developing a Lighter, Stronger, and Cleaner Air-Melt Steel for Critical Applications

Steel components, particularly those used in critical applications such as bearings and fuel injection systems, are increasingly expected to be […]

Advantages of Direct Gear Design For Automotive Polymer Gear Drives

Invention of the gear-generating machining process that uses the gear rack shape tooling cutting edge (as shown in Figure 1) […]

A Comparison of Wrought Steel Gears and Surface – Densified Powder Metallurgy Gears