Paulo’s Kansas City Facility Now NADCAP Approved

0
1969

In a recent press release Paulo Products Company announced that its Kansas City, Missouri, facility has been awarded accreditation to the National Aerospace and Defense Contractors Accreditation Program. NADCAP was developed in cooperation with the DOD, SAE, and ASTM to certify and accredit suppliers via a third-party audit program administered by the Performance Review Institute. Paulo-Kansas City joins American Brazing-Willoughby, Ohio–a division of Paulo–in the NADCAP program.

Paulo-Kansas City is unique in that it offers conformance to NADCAP heat-treat standards in large continuous belt equipment as well as atmosphere batch and vacuum equipment. This significant achievement is a reflection of Paulo’s commitment to leadership in the technical, operational, and quality initiatives in the aerospace, defense, and other market sectors.

Doug Manning, division sales manager for Paulo-Kansas City, says that "The NADCAP accreditation process is extremely rigorous and involves everyone in the facility. We recognized our customers need for us to have NADCAP accreditation and we all pulled together to meet that need."

Paulo provides a wide variety of innovative engineered solutions in heat treating, brazing, and metal finishing. Paulo-Kansas City is one of the largest and most complete heat-treating facilities in the region, specializing in vacuum, batch, induction, and large continuous belt heat treating. Paulo also offers its customers a broad range of metallurgical services and extensive engineering resources. In addition to the Kansas City plant, Paulo operates facilities in Willoughby, Ohio; St. Louis, Missouri; and Nashville and Murfreesboro, Tennessee.

For more information contact Manning at (816) 861-7500 ext. 206 or dmanning@paulo.com. The company’s Web site is [www.paulo.com].