AMClad tooling is 3D printed in low-cost sand on ExOne systems and then infiltrated and coated using Freshmade 3D’s patented method. (Courtesy: ExOne)

The ExOne Company, a global leader in industrial sand and metal 3D printers using binder jetting technology, has acquired the assets of Freshmade 3D, an Ohio-based startup with a patented method of creating durable AMClad® tooling out of sand forms 3D printed on ExOne machines.

The strategic move will strengthen ExOne’s position as a provider of large-format 3D printed tooling for industrial applications.

AMClad tooling, which is 3D printed in low-cost sand on ExOne systems and then infiltrated and coated using Freshmade 3D’s patented method, often eliminates weeks or months of time spent waiting for conventional tooling, and typically offers a 30-50 percent cost saving.

This fast, durable, and affordable solution can be used for a wide range of tooling applications, including composite layup, vacuum forming, compression molds, urethane casting molds, trim fixtures, hydroforming, sheet metal stamping, and more. AMClad tooling is being used today by customers in the aerospace, art, architecture, automotive, construction, and energy industries. 

ExOne has been developing tooling products for its large, industrial 3D printers since 2014, and offers sacrificial tooling for composite layup that washes out with water. However, ExOne believes Freshmade 3D’s patented approach offers additional unique benefits and can help accelerate adoption of 3D printed sand tooling solutions.

“We are delighted to add Freshmade 3D’s patented process for creating durable 3D printed tooling to our portfolio,” said John Hartner, ExOne CEO. “We plan to scale up this process for a global aerospace customer, who intends to use this tooling for composite layup of parts. This is an ideal solution for companies looking to shorten supply chains and produce tooling and final products locally.”

“We launched AMClad with the idea of using sand 3D printing technology to deliver hard tooling faster and with more design freedom, to enable U.S. manufacturers to produce more locally and faster,” said Rich Wetzel, Freshmade 3D co-founder, who will now join ExOne’s applications team. “ExOne is the best company to accelerate this technology as we scale up for customers who’ve decided to leverage our solution to meet production goals faster. Companies are just beginning to discover how robust and affordable this technology is over conventional tooling.”

In addition to tooling, the AMClad process is being used to produce artwork or restoration pieces, including replication statues for museum exhibits, exterior reproductions for architectural refurbishment, or custom chrome details on classic cars. The versatile surface finishes available with the AMClad process include metal, stone, or painted finishes that allow for a range of artistic applications to be realized in a cost-effective manner.

Freshmade 3D was founded by Wetzel, Christoper Tomko, and Dr. Brett Conner in 2016 and is a portfolio company of the Youngstown Business Incubator, which supports the development of innovative high-tech companies in the Northeast Ohio region. Freshmade 3D has also received development support from America Makes, part of the National Network for Manufacturing Innovation established by the Revitalize American Manufacturing and Innovation Act of 2014.

“We’re so proud to be a part of Freshmade 3D’s success,” said Barb Ewing, CEO of the Youngstown Business Incubator. “Two of the three founders started their entrepreneurial career as part of our team.  They are proof that northeast Ohio is fast becoming the epicenter for additive manufacturing in North America.”