PRODUCT SHOWCASE: DiaCut CP Punching Oils From Oelheld

0
5510

DiaCut CP punching oils have been developed especially for fast punching machines. They effectively prevent the formation of built-up edges and allow for punching largely without burrs. DiaCut CP punching oils are rolled or sprayed onto the work pieces to be processed. After the operation, the parts are practically free of residue. DiaCut CP punching oils are free of chlorine and heavy metals and practically free of aromatic compounds, so they guarantee the best health protection as well as greatest possible performance.

DiaCut CP 1
A punching oil of highest purity, developed for steel and non-ferrous heavy metals. All of the ingredients have been admitted for contact with food by the American Food and Drug Authority (FDA). DiaCut CP 1 is extremely thin-bodied and evaporates without leaving any residue behind.

DiaCut CP 2
A punching oil with low viscosity and good performance, suitable for steel and copper alloys. It evaporates leaving practically no residue behind.

DiaCut CP 3
A thin-bodied highly effective punching oil with very good EP qualities for the processing of steel and copper alloys. DiaCut CP 3 can also be used as a drawing oil, which leaves practically no residue behind. At the same time, it offers increased protection against corrosion for longer storage of the processed parts.

DiaCut CP 5
A very highly alloyed punching oil that can nevertheless be used for copper alloys (except for very pure copper).

DiaCut CP 6
A highly alloyed punching oil for nickel chromium steel, also suitable as a drawing oil. DiaCut CP 6 is thin-bodied, it evaporates leaving practically no residue behind, and it affords an increased protection against corrosion. It is not suited for copper alloys.

For further information, contact oelheld U.S. at (847) 531-8501 or visit their website at www.oelheld.com.