New Fullcut Mill FCR Type from BIG Kaiser

0
1309

BIG Kaiser Precision Tooling, Inc., introduces Fullcut Mill FCR Type, a new indexable insert endmill that tests conclude has five times greater DOC capability and lower cutting resistance than three competitor’s tools.

The new FCR’s geometry expands capabilities in multi-functional milling, achieving supreme performance for ramping, helical-, shoulder-, and plunge-milling operations. The sharp cutting edges of the unique indexable insert retain high strength and toughness due to the optimized eccentric relief angle for each cutter diameter. Extremely sharp cutting edges with both high radial and axial rake angles achieve smooth and quiet endmilling in all materials. Fullcut Mill FCR is available for diameters 5/8”, 3/4”, 1”, and 1 ¼” in various length configurations with BIG PLUS integral shanks CAT40, BT30, and BT40 as well as HSK-A50 and A63 versions.

For more information call (888) TOOL-PRO/866-5776, send e-mail to bigkaiser@bigkaiser.com, or go to [www.bigkaiser.com].