E-Z Lok offers threaded press-in inserts for plastics

0
3840
E-Z Lok E-Z Press™ inserts are designed for post-molding installation in either thermoset plastics or thermoplastics. (Courtesy: E-Z Lok)

E-Z Lok, a leading manufacturer and master distributor of threaded inserts for metal, plastic, and wood, offers E-Z Press™ inserts.

Press-in Inserts are designed for post-molding installation in either thermoset plastics or thermoplastics. A slotted design with diamond-knurled OD allows for “cold” installation with optimum torque/pull-out resistance. When the E-Z Press insert is installed, it compresses slightly along the slot. As the fastener is threaded into place, the insert expands and the diamond knurl is pressed into the wall of the hole, securing the insert in place. 

Cold installation of threaded inserts reduces the costs of moldings and eliminates the need to “chase” threads after molding. Furthermore, they also help cut reject waste caused by misaligned and faulty in-serts and assist in proper installation without a precise hole depth.

E-Z Press inserts are available in three styles: flush, flanged, and reverse slot. All three types press into place for fast, easy installation. Anything from a rubber mallet to an arbor press can be used for installa-tion.

CAD files on this product can be downloaded in more than 100 file formats from the E-Z Lok website.

E-Z Lok is a leading manufacturer and master distributor of threaded inserts for metal, plastic and wood. Inserts for metal include solid wall and helical wire-thread inserts, while inserts for plastic feature press-in and ultrasonic/heat stake designs. Those for wood are die cast zinc alloy hex drives for soft wood and brass knife threads for hard wood. A variety of kits for the above inserts are available and feature installation tools, drill bits, etc.

E-Z Lok is a third-generation family-owned and operated company. Founded in 1956, it primarily sells through local, regional, and national industrial distributors.

MORE INFO  www.ezlok.com