The Next Dimension in Detecting Tooth Distortion
The conventional CNC gear inspection machine will measure and evaluate helix and involute tooth flank deviations that are relative to […]
Material Benefits at 300 Below
For decades, cryogenic treatment has been one of metalworking’s best-kept secrets. It has become mainstream in recent years, and it […]
The Simultaneous Dual Frequency Method of Inductive Gear Hardening
Inductive surface hardening is an attempt to harden only the surface of a structure without affecting the inner portions of […]
Manufacturing Single-Envelope Worm Gears
First, the basics. Worm gear sets are used to transmit power between non-parallel, non-intersecting shafts, usually having a shaft angle […]
High Performance Gear Cuts a Path to Stronger Bevel Gears
Faced with ever-increasing horsepower and torque requirements, in conjunction with size constraints, High Performance Gear (HPG) began investigating ways to […]