Pre-Nitriding: A Means of Significantly Increasing Carburizing Throughput

Pre-nitriding is a technology that addresses grain growth and creates a finer grain structure in the carburized case at higher temperatures. Case studies show how carburizing productivity has doubled, and sometimes tripled, using pre-nitriding.