Contour Hardening Bevel, Hypoid, and Pinion Gears

TSH technology is an advanced induction hardening process that was specifically developed to reduce overall cost and to replace thermo-chemical heat treating processes.

Induction Gear Hardening

Part 1: The practice and science of modern induction heat-treating has advanced in many areas over the last decade, including computer modeling, power supplies, failure analysis, quality assurance, and more.

Induction Gear Hardening: Part 2

The second in a two-part series, this installment addresses induction gear hardening by encircling the whole gear or sprocket with an induction coil, also known as ‘spin hardening.’